This work reports the result of the thermo-mechanical investigations carried out on strain-hardened NST 37-2 a Nigerian low carbon steel that has a wide industrial applications; the objective being to improve the drawability of this grade of steel.

NST 37-2 is strain-hardened by wire-drawing from 6mm diameter rolled product to 5mm (30.56% reduction), 4mm (55.56% reduction), 3mm (75% reduction), and 2mm (88.89% reduction). Mechanical properties-yield strength, ultimate tensile strength, hardness, per cent elongation and per cent reduction in area are determined on the test pieces before and after the wire drawing (strain-hardening) operations. This is followed by sub-critical annealing at annealing temperatures of 500°C and 650°C. Microstructural investigations are carried on the strain-hardened and annealed test pieces.

For optimum drawability NST 37-2 should not be strain-hardened beyond 75% reduction and the strain-hardened steel should be sub-critically annealed at 650°C annealing temperature for 15 minutes.