Engineering properties of Amuro-Okigwe fired day bricks were studied. Chemical composition of the day revealed a high SiO2, content. Firing of the bricks took place from 7500C to 10500C. The bricks exhibited high percentage of plasticity and the shrinkage limit was between 1.790 to 4.270 percent. The bulk density was between 1.77 and 1.94g/cm3 The water absorption was between 11.57 and 18.92 percent. The Modulus of Rupture was in the range of 1287 and 3819 Pa. The properties of high SiO2, content, bulk density and water absorption are appropriate for building.